hot products

NCM-811 Lithium-Ion Secondary Battery Cathode Material

Wechat:J15750811203

Skype and Whatsapp :+86 15750811203

Email: Daisy@foam-material.com

  • item no :

    ZOPIN-NCM811
  • moq :

    1
  • lead date :

    In Stock
  • payment:

    Credit Card L/C D/A D/P T/T Western Union
product details

NCM-811 Lithium-Ion Secondary Battery Cathode Material 



Introduction

NMC811 is a lithium-ion battery cathode material with the chemical formula LiNiMnCoO2. This chemical composition indicates that the cathode material contains nickel (Ni), manganese (Mn), cobalt (Co), and lithium (Li). The numerical part "811" represents its ratio, where the proportions are in a molar ratio of 8:1:1 for Ni, Mn, and Co, respectively. This cathode material is commonly used in high-energy-density lithium-ion batteries to enhance the overall performance of the battery.

 

1. NMC-811-S (single crystal Ni83) physical and chemical indicators

Product Name

D50

μm

surface area

m2/g

pH

LiOH

wt%

Li2CO3

wt%

3.0-4.3V

0.1C

charge capacity mAh/g

Initial Discharge Efficiency %

Features

NMC-811-S

4.0±1.0

0.6±0.2

≤11.7

≤0.30

≤0.30

210±5

89±1

High safety, high capacity, excellent circulation

Typical value

3.6

0.65

11.50

0.21

0.09

210.2

89.6

2. Coin cell performance

1Room temperature performance(3-4.3V)

Product

Room temperature performance (3-4.3V)

0.1/0.1C

0.5/0.5C

0.5/1C

0.5/2C

0.5/1C

First charge

(mAh/g)

First discharge

(mAh/g)

Initial efficiency

(%)

3th Capacity

(mAh/g)

4th Capacity

(mAh/g)

5th Capacity

(mAh/g)

6th Capacity

(mAh/g)

55th Capacity

(mAh/g)

50th Capacity retention

(%)

NMC-811-S

234.5

210.2

89.6

196.7

190.5

183.5

190.2

174.5

91.7

 

2)High temperature 45℃ power-withholding performance (3-4.3V)

Product

 45℃ performance (3-4.3V)

0.1/0.1C

0.5/0.5C

0.5/1C

0.5/2C

0.5/1C

First charge

(mAh/g)

First discharge

(mAh/g)

Initial efficiency

(%)

3th Capacity

(mAh/g)

4th Capacity

(mAh/g)

5th Capacity

(mAh/g)

6th Capacity

(mAh/g)

55th Capacity

(mAh/g)

50th Capacity retention

(%)

NMC-811-S

242.2

222.2

91.7

213.8

208.1

201.6

206.3

191.9

93

 

3. Application of single crystal Ni83 full battery:

1Battery design (pouch cell 554065 2.1Ah):

Positive NMC-811-S

Negative S360-L1

Design specific capacity (mAh/g)

Area density g/m2

Compaction density

g/cm3

Design specific capacity

mAh/g)

Area density(g/m2

Compaction density (g/cm3

Anode excess

200

330

3.6

350

218

1.65

12%

 

Positive

active substance

SP+GNLC-05

Solef5130

Actual solid content

Viscosity/temperature

NMC-811-S

97.30%

0.5%+1.0%

1.20%

73.00%

6030/25.4

Negative

active substance

SP

Dazhalu 2200

SBR(104A)

Actual solid content

Viscosity/temperature

S360-L1

95.20%

1.50%

1.30%

2.00%

42.70%

3570/26.9

 

2)Compaction performance

pressure level(Mpa)

5

6

7

8

9

10

NMC-811-S

3.2

3.33

3.37

3.4

3.45

3.53

 





NCM






related products

Copyright © Cheap Copper Foam, Iron Nickel Foam, Titanium Foam All Rights Reserved. Powered by dyyseo.com